Fig. 14: SEM images of the ‘Dot’ sample after testing.
From: Effect of salt deposition patterns on stress corrosion cracking

a-c Corresponds to varying salt flux (1.2 μg/cm2/h, twice, and four times as much respectively). The analysis demonstrates that as salt flux increases the area of salt dispersion also increases.