Extended Data Fig. 5: Simulated fracture characteristics.
From: Flexible solar cells based on foldable silicon wafers with blunted edges

Together with the increase of Rp from 0 to 15.81 nm, the fractured path dually becomes more tortuous at a strain of 27.5%. Some jagged notches are also observed, in consistent with experimental results in Extended Data Fig. 4b.