Extended Data Fig. 5: Oxide scale and near-surface region of Cr-37.2Mo AC after 100 h of oxidation at 800 °C.
From: A ductile chromium–molybdenum alloy resistant to high-temperature oxidation

a, SEM-EDS. b, Schematic.
From: A ductile chromium–molybdenum alloy resistant to high-temperature oxidation
a, SEM-EDS. b, Schematic.