Table 1 Parameters of the tested samples of different zinc concentration x.

From: Topological Phase Transition in Single Crystals of (Cd1−xZnx)3As2

x

0.00

0.07

0.13

0.29

0.31

0.38

Parameters

AF(10−3 Å−2)

8.08

6.18

2.53

1.30/1.74

1.98

2.66/4.01/6.66

kF−1)

0.051

0.044

0.028

0.02/0.024

0.025

0.029/0.036/0.046

EF(eV)

0.346

0.289

0.165

0.107/−

0.143

0.169/−/−

νF(105 m/s)

9.9

10.1

9.1

8.3/−

8.6

9.4/−/−

m*(me)

0.061

0.051

0.036

0.028

0.034

0.036

  1. The dashed entries mean quantities missing.