Table 2 Carrier concentration and the mobility of Ce-doped AgSb1−xCexTe2 samples.
From: Enhanced thermoelectric properties of AgSbTe2 obtained by controlling heterophases with Ce doping
Sample | h (/cm3) | μ (cm2/Vs) |
|---|---|---|
AgSbTe2 | 5.55 × 1018 | 190 |
x = 0.001 | 6.59 × 1018 | 163 |
x = 0.002 | 1.32 × 1019 | 143 |
x = 0.003 | 1.27 × 1019 | 175 |
x = 0.004 | 1.57 × 1019 | 157 |