Figure 1 | Scientific Reports

Figure 1

From: Nanocrystalline diamond protects Zr cladding surface against oxygen and hydrogen uptake: Nuclear fuel durability enhancement

Figure 1

(a) weight gains (mg/dm−2) measured after 6, 15, 30, 90, 120, 150, 170 and 195 days of exposure to hot water (360 °C) for uncoated and 300 nm NCD-coated ZIRLO plate samples. (b) weight gains (mg/dm−2) measured after 6, 15, 20, 30, 40 and 90 days of exposure to hot water (360 °C) for uncoated, 300 nm NCD-coated, 500 nm NCD-coated and 700 nm NCD-coated ZIRLO plate samples. Thicker NCD layers provide ZIRLO plates with stronger protection against oxidation than thinner layers do.