Table 1 Properties of each of the three grain boundaries.
From: Multiscale correlative tomography: an investigation of creep cavitation in 316 stainless steel
Grain boundary | Cavitated? | Angle to direction of principal stress | Crystallographic Misorienation |
---|---|---|---|
1–2 | Yes | 62° | 58° |
1–3 | Yes | 63° | 45° |
2–3 | No | 31° | 35° |