Figure 2

Total structure factors, S(Q), for the 75Li2S-25P2S5 glasses obtained from X-ray diffraction before annealing and after annealing at 120 °C, 180 °C, 200 °C, 240 °C, and 270 °C.

Total structure factors, S(Q), for the 75Li2S-25P2S5 glasses obtained from X-ray diffraction before annealing and after annealing at 120 °C, 180 °C, 200 °C, 240 °C, and 270 °C.