Table 1 Paper samples characteristics.

From: Occurrence of temperature spikes at a wetting front during spontaneous imbibition

Paper type

porosity

Mean pre size

Layer(s)’s material

Thickness

Ziegler

52%

10 µm

Cellulose

120 µm

Coated paper (Magno glass)

   Coating layer

34%

180 nm

CaCO3

10 um

   Fibrous layer

50%

(2×)10 um

Cellulose

65 um

RL 200

50%

12 µm

Cellulose

260 µm

RL professional

48%

12 µm

Cellulose

340 µm

Plastic based

65%

16 µm

Plastic

220 µm

Prematex

60%

20 µm

Cellulose

300 µm