Figure 7

Stress-induced leakage current characteristics of (a) as-grown HfO2/InSb, (b) post-annealed HfO2/InSb at 400 °C, (c) as-grown HA/InSb, and (d) post-annealed HA/InSb at 400 °C.
Stress-induced leakage current characteristics of (a) as-grown HfO2/InSb, (b) post-annealed HfO2/InSb at 400 °C, (c) as-grown HA/InSb, and (d) post-annealed HA/InSb at 400 °C.