Figure 4

Variation of deposition rate of the L-PPA:N coatings as a function of (a) N2 gas flow rate in different powers and (b) RF power in 40 sccm (C2H2 flow rate: 20 sccm).

Variation of deposition rate of the L-PPA:N coatings as a function of (a) N2 gas flow rate in different powers and (b) RF power in 40 sccm (C2H2 flow rate: 20 sccm).