Figure 2
From: The High Temperature Tensile and Creep Behaviors of High Entropy Superalloy

(a) The typical γ/γ′ microstructure of HESA and (b) the XRD characteristic peaks of γ and γ′ phases. (c) The DTA curve during heating after solution and aging heat treatments. (d) Deconvolution of {200} reflection of HESA at 982 °C.