Figure 2

Physiochemical characterization of ZnO nanoparticles milled at different time. (A) Structural determination by XRD analysis at 200–800 2Ѳ (Inset shows diffraction intensity between 300–400 (B) Optical characterizations by UV-Vis spectroscopy showing SPR peak shift with increase in milling time.