Figure 4

XRD spectra for the ITO film on glass substrate, fresh sample and 1000 hrs aged sample. The table given in the inset shows that line boarding decreased and grain size is increased in the aged sample.

XRD spectra for the ITO film on glass substrate, fresh sample and 1000 hrs aged sample. The table given in the inset shows that line boarding decreased and grain size is increased in the aged sample.