Table 1 Encapsulation efficiency, loading and desorption capacity, size and zeta potential of the prepared NPs.
Sample | %LC | % Encaps | %Des | Size (nm) | Zeta potential (mV) |
|---|---|---|---|---|---|
LPO-loaded NPs | 62.49 ± 0.09 | 88.9 ± 0.12 | — | 214.7 ± 16 | 50.5 |
LPO coated NPs | — | — | 76.68 ± 0.8 | 297 ± 8 | 16.8 |
LF-loaded NPs | 64.38 ± 0.62 | 91.6 ± 0.88 | — | 228.5 ± 9.5 | 51 |
LF coated NPs | — | — | 96.84 ± 0.65 | 323.5 ± 7.5 | 17.7 |
LPO + LF-loaded NPs | 58.5 ± 0.56 | 83.29 ± 0.8 | — | 389 ± 11 | 51.4 |
LPO + LF coated NPs | — | — | 94.78 ± 0.22 | 507 ± 18 | 10.9 |
LF coat LPO-loaded NPs | 62.3 ± 0.92 | 88.7 ± 1.3 | 96.7 ± 0.3 | 477.5 ± 12.5 | 20.6 |
LPO coated LF-loaded NPs | 64.18 ± 0.37 | 91.3 ± 0.53 | 75.6 ± 0.65 | 460.5 ± 10.5 | 19.9 |