Table 2 Phonon mode frequencies (cm−1) at Γ point in La7Ir3. I: infrared active, R: Raman active.

From: Evidence of s-wave superconductivity in the noncentrosymmetric La7Ir3

Γ(0, 0, 0)

E1(I + R)

0

32.1

54.6

62.6

75.8

81.9

91.3

100.5

108.2

135.4

E2(R)

38.6

45.7

58.4

63.1

68.1

81.7

93.9

98.7

103.3

117.3

A1(I + R)

0

38.1

74.3

91.1

93.9

97.3

116.4

   

A 2

27.5

65.0

101.0

       

B 1

51.9

61.7

99.5

       

B 2

54.2

80.1

86.2

90.2

105.9

107.0

138.0