Figure 5

Retention characteristics of the h-BN/Cu stack across six different locations. After the probed locations are stressed to LRS, these locations are subjected to small read voltage lying in the range of 100 mV to 1 V. Self-recovery was consistently observed in time scales of ~10–100 sec and the probed location returned to the HRS state.