Figure 4
From: Thermally Stable, High Performance Transfer Doping of Diamond using Transition Metal Oxides

Hall measurements over time for MoO3 (Sample D) and V2O5 (Sample I) doped H-diamond samples with a 400 °C in-situ anneal prior to deposition.