Figure 2
From: Reversible 90-Degree Rotation of Fe Magnetic Moment Using Hydrogen

(a) AFM topography images and line profiles of a pristine MgO(001) before (a) and after 700 °C thermal annealing (b).
From: Reversible 90-Degree Rotation of Fe Magnetic Moment Using Hydrogen
(a) AFM topography images and line profiles of a pristine MgO(001) before (a) and after 700 °C thermal annealing (b).