Figure 4

In-situ X-ray diffraction (XRD) patterns for Co6 alloy in the range 35° < 2θ < 50° during cooling (a) from 343 K to 283 K and (b) from 273 K to 173 K, respectively. The diffraction peaks marked by five-pointed star corresponds to the sample stage.