Table 2 Thermal conductivity measurements of diamond/Al composites.
From: Enhanced bending strength and thermal conductivity in diamond/Al composites with B4C coating
Sample | Density (g/cm3) | Specific heat (J/g·K) | Thermal diffusivity (mm2/s) | Thermal conductivity (W/m·K) |
---|---|---|---|---|
D1 | 2.86 | 0.76 | 95.9 | 208.4 |
D2 | 2.92 | 0.71 | 115.9 | 240.3 |
D3 | 2.96 | 0.67 | 144.4 | 286.4 |
B1 | 2.92 | 0.77 | 139.0 | 312.5 |
B2 | 2.99 | 0.73 | 152.3 | 332.4 |
B3 | 3.04 | 0.69 | 168.6 | 353.7 |