Table 1 Parameters of pristine TiO2 and TiOxNy coated TiO2 powders.
Sample | a0 (Å) | c0 (Å) | Crystallite size (nm) | BET surface area (m2/g) |
---|---|---|---|---|
TiO2 | 3.78 | 9.54 | 19.03 | 112.6 |
TiO2@20TiN | 3.78 | 9.55 | 19.27 | 112.6 |
TiO2@50TiN | 3.78 | 9.53 | 18.98 | 111.7 |
TiO2@100TiN | 3.78 | 9.55 | 18.55 | 115.2 |