Table 1 Microbial activity of ACDC at various Cl − NO3 combinations and ionic strengths (µ).

From: Nitrite producing bacteria inhibit reinforcement bar corrosion in cementitious materials

µ (M)

Cl (M)

NO3 (M)

HCOO (M)

Na+ (M)

NO3 reduction ratea (mmol.g−1.d−1)

NO2 accumulation ratea (mmol.g−1.d−1)

0.70

0.30

0.20

0.20

0.70

2.70 ± 0.01

2.30 ± 0.25

0.80

0.30

0.30

0.20

0.80

1.40 ± 0.15

1.00 ± 0.15

0.40

0.20

0.20

0.80

1.00 ± 0.10

0.90 ± 0.15

0.90

0.40

0.30

0.20

0.90

0.55 ± 0.25

0.40 ± 0.20

0.50

0.20

0.20

0.90

0.80 ± 0.20

0.60 ± 0.15

1.00

0.40

0.40

0.20

1.00

0.80 ± 0.05

0.65 ± 0.10

0.50

0.30

0.20

1.00

0.70 ± 0.05

0.50 ± 0.20

1.10

0.50

0.40

0.20

1.10

0.55 ± 0.10

0.30 ± 0.05

1.20

0.50

0.50

0.20

1.20

0.30 ± 0.10

0.15 ± 0.02

  1. ap = 0.05, statistical significance calculated by one way ANOVA and obtained from three replicate experiments.