Table 1 Physicochemical and mechanical evaluations of hydrophobically modified alginate-psyllium husk gel composite film.

From: Preparation of Lauroyl Grafted Alginate-Psyllium Husk Gel Composite Film with Enhanced Physicochemical, Mechanical and Antimicrobial Properties

Concentration (in % w/v)

Thickness (in mm) study in triplicate

Weight variation (in g) study in triplicate

Folding endurance (no. of times)

% Elongation study in triplicate

% Swelling study in triplicate

In vitro deformation (in min) study in triplicate

4% Psyllium gel

1.40 ± 0.1

0.035 ± 0.002

128 ± 0.01

6.32 ± 0.03

NA

NA

4.75 (4% Psyllium gel + 0.75% alginate)

0.35 ± 0.02

0.472 ± 0.01

135.33 ± 0.57

24.28 ± 0.02

14.30 ± 0.02

5.5 ± 0.01

5 (4% Psyllium gel + 0.75% alginate + 0.25% lauryl grafted alginate)

0.37 ± 0.02

0.481 ± 0.001

137 ± 0.01

27.28 ± 0.02

15.39 ± 0.03

5.9 ± 0.05