Figure 3
From: Low-pressure-responsive heat-storage ceramics for automobiles

Time evolution of the thermographic image on applying pressure to block-type λ-Ti3O5. Snapshots taken from the thermogram of the sample on applying pressure as observed by thermography. Pressure is applied to the sample at t = 0. The sample temperature reached a maximum of 85.5 °C.