Figure 4 | Scientific Reports

Figure 4

From: Growing a LaAlO3/SrTiO3 heterostructure on Ca2Nb3O10 nanosheets

Figure 4

(a) IV-curves before (blue, bottom) and after (red, next curve up) annealing, taken on sample B. For comparison, two IV-curves taken on an STO substrate are also shown, one TiO2 -terminated (green, 2nd from top) and one SrO -terminated (magenta, top). Curves are shifted for clarity. (b) Intensity and (c) FWHM versus landing energy during the annealing process. The dotted line marks the time from which the temperature was kept constant after ramping up. The FWHM is given in percentage of the Brillouin zone. Figure taken from16.