Figure 11
From: Thermal damage of tungsten-armored plasma-facing components under high heat flux loads

Equivalent plastic strain on the path A-M after the application of transient loads for 0.2 ms, 0.6 ms and 1.0 ms. Steady-state load is 6 MW/m2 (left). Steady-state load is 12 MW/m2 (right).