Figure 8
From: Thermal damage of tungsten-armored plasma-facing components under high heat flux loads

Crack initiation time of 16 MW/m2. Temperature contour plots (left) and maximum principal stress contour plots (right).
From: Thermal damage of tungsten-armored plasma-facing components under high heat flux loads