Table 1 Mean size of chitosan particles prepared under various precursor concentrations in a fixed flow rate of air: 0.075 L/min and inlet temperature (Tc): 130 °C.
Sample code | Chitosan (%,w/v) | TH (%,w/v) | TPP (% w/v) | Mean Size (nm) | G.S.D (σg) |
|---|---|---|---|---|---|
C1 | 5 × 10−5 | 0 | 0 | 98 | 1.28 |
C2 | 5 × 10−4 | 101 | 1.27 | ||
C3 | 5 × 10−3 | 174 | 1.12 | ||
C4 | 0.01 | 185 | 1.17 | ||
C5 | 0.05 | 280 | 1.17 | ||
C6 | 0.1 | 415 | 1.19 |