Figure 6 | Scientific Reports

Figure 6

From: Stacking Fault Energy Analyses of Additively Manufactured Stainless Steel 316L and CrCoNi Medium Entropy Alloy Using In Situ Neutron Diffraction

Figure 6

BF-STEM images along the 〈101〉 zone axis showing dislocations in as built (a,b) and multiple slip systems in deformed (engineering strain, ε = 58%) with LSR (2 × 10−5 s−1) (c,d) AM CrCoNi alloy. Marked twin spots in selected area diffraction (SAD) pattern (e) taken at the red circle in (d). Note that (f) is taken from deformed (ε = 47%) with HSR (2 × 10−3 s−1) AM CrCoNi alloy specimen.