Table 1 Controlling parameters for successful CNT/5E2N microencapsulation.

From: Recovery of electro-mechanical properties inside self-healing composites through microencapsulation of carbon nanotubes

Parameters

Amounts

CNT

0.1 wt. %

Sonication power

6 W

Sonication time

2 h and 30 min

Stirring speed

700 rpm

PVA

6.3 wt. %, Molecular weight: 85000–124000

SLS

0.75 wt. %