Table 4 Reported values of DSSC devices using Barium Stannate and porphyrin/N719 dye.

From: Efficient light harvesting using simple porphyrin-oxide perovskite system

#

Material type

BSO morphology

Sensitization duration

Voc (V)

η (%)

FF (%)

Ref

1

Barium stannate + N719

Nanoparticles

24 h

0.68

1.1

60

13

2

Barium stannate + N719

Nanoparticles

0.6

5.2

66

16

3

Barium stannate + TiCl4 + N719

Nanoparticles

60 min

0.62

6.2

64

5

4

Barium stannate + TiCl4 + N719

Nanorods

20 min

0.8

6.86

54

4

5

Barium Stannate + TiCl4 + Porphyrin

Microrods

30 min

0.6

6.1

81

Present work