Figure 2 | Scientific Reports

Figure 2

From: Role of Al in Na-ZSM-5 zeolite structure on catalyst stability in butene cracking reaction

Figure 2

1H, 27Al, and 29Si MAS NMR of Na-ZSM-5 catalysts with different SiO2/Al2O3 molar ratios (ac) 1H MAS NMR of fresh Na-ZSM-5 catalysts with the SiO2/Al2O3 molar ratios = 20, 35, and 50, respectively, (df) 27Al MAS NMR of fresh Na-ZSM-5 catalysts with the SiO2/Al2O3 molar ratios = 20, 35, and 50, respectively, (gi) 27Al MAS NMR of spent Na-ZSM-5 catalysts with the SiO2/Al2O3 molar ratios = 20, 35, and 50, respectively, jl29Si MAS NMR of fresh Na-ZSM-5 catalysts with the SiO2/Al2O3 molar ratios = 20, 35, and 50, respectively, and (mo) 29Si MAS NMR of spent Na-ZSM-5 catalysts with the SiO2/Al2O3 molar ratios = 20 ,35, and 50, respectively.

Back to article page