Table 1 The mean diameter (SEM), the hydrodynamic hydrometer (DLS) and the polydispersity index (PDI) values for the various PLGA-PEG microspheres formulations.

From: Drug-encapsulated blend of PLGA-PEG microspheres: in vitro and in vivo study of the effects of localized/targeted drug delivery on the treatment of triple-negative breast cancer

Formulation

SEM (μm)

DLS (μm)

PDI

PLGA-PEG

0.80 ± 0.26

3.14 ± 0.09

0.82

PLGA-PEG_PGS

1.23 ± 0.18

5.44 ± 0.23

0.67

PLGA-PEG_ PGS-LHRH

1.16 ± 0.18

6.92 ± 0.44

0.47

PLGA-PEG_PTX

0.88 ± 0.18

5.26 ± 0.53

0.58

PLGA-PEG_PTX-LHRH

1.03 ± 0.37

6.02 ± 0.80

0.39