Figure 2

(a) Change of relative resistance (R/R0) of ISHCP, with different conditions, coated on SEBS substrate under 0 to 50% strain. (b) Variation of the relative resistance and electrical conductivities of optimized ISHCP coated on SEBS substrate as a function of the strain. (c) Demonstration of deformable ISHCP coated on a SEBS substrate with stretch-release under 400% strain.