From: Hydrometallurgical process development to recycle valuable metals from spent SCR deNOX catalyst

Effects of temperature at the time of roasting process (s = solid, aq = aqueous) in the (a) leaching of vanadium and tungsten and (b) in the concentration of Si leached.