Table 7 Trials batches of SCC.

From: RETRACTED ARTICLE: Performance of sustainable self-compacting fiber reinforced concrete with substitution of marble waste (MW) and coconut fibers (CFs)

Materials

Mix 1

Mix 2

Mix 3

Mix 4

Mix 5

Mix 6

Mix 7

Mix 8

Cement (kg/m3)

425

425

425

425

425

425

425

425

Sand (kg/m3)

625

625

625

625

625

625

625

625

Coarse Aggregate (kg/m3)

1270

1270

1270

1270

1270

1270

1270

1270

Water cement ratio (W/C)

0.50

0.50

0.50

0.50

0.60

0.60

0.60

0.60

Superplasticizer (kg)

2.12

4.25

6.37

2.12

4.25

6.37