Figure 3

Representative SEM images [with increasing magnification from (a) to (b)] of the nanoporous Au particles obtained by HNO3 dealloying of the alloy Au–Ag particles obtained on the FTO surface after irradiating the Ag-Au bilayer by laser fluence 1.0 J/cm2.