Table 2 Materials used for testing.
Designation | Input material | Chemical treatment of powder | Processing |
|---|---|---|---|
Mg_HF_SPS | Mg powder | HF (24 h) | Cold pressing and SPS (500 °C) |
Zn_SPS | Zn powder | – | Cold pressing and SPS (300 °C) |
Zn0.8 Mg | Zn, Mg ingots | – | Casting (on air) + extrusion (300 °C and extrusion ratio 10) |