Table 2 Statistical data of DSC for PBS and PBS/PTFE composites.

From: The effect of polytetrafluoroethylene particle size on the properties of biodegradable poly(butylene succinate)-based composites

Samples

\({\mathrm{T}}_{\mathrm{c}}\) (℃)

\({\mathrm{T}}_{\mathrm{m}}\) (℃)

\(\Delta {\mathrm{H}}_{\mathrm{c}}\) (J/g)

\(\Delta {\mathrm{H}}_{\mathrm{m}}\) (J/g)

\(\Delta {\mathrm{H}}_{\mathrm{cc}}\) (J/g)

\({\mathrm{X}}_{\mathrm{c}}\) (%)

PBS

78.2

113.9

70.2

85.9

10.7

37.6

PBS/P220

85.7

114.5

72.8

81.8

4.5

39.8

PBS/P5

86.1

114.2

76.8

85.1

6.2

40.7

PBS/P500

91.8

116.3

78.2

86.8

44.8