Figure 2
From: Mid-wavelength infrared avalanche photodetector with AlAsSb/GaSb superlattice

(a) The atomic force microscopy image of the grown MWIR APD sample over 10 μm × 10 μm area. (b) HR-XRD scan curve of the grown APD sample, where peaks of different regions are marked.