Figure 1 | Scientific Reports

Figure 1

From: Laser induced crystallization of Co–Fe–B films

Figure 1

XRD θ-2θ scans of Co40Fe40B20 with a Ta capping layer furnace annealed for 30 min at temperatures in the range from 400 °C to 550 °C (a), and at 450 °C for different annealing durations (b). The vertical coherence lengths determined from the CoFe(110) reflex for both Co–Fe compositions are shown in the insets.