Figure 2

(a–f) Electro-spun lignin fibres using 95%ASL–5%ESL in acetone/DMSO: (a) macroscopic appearance of the deposition area (randomly oriented fibres); and (b–f) magnified SEM micrograph of fibres produced using the 52.8 wt% total polymer solution concentration.