Figure 3
From: Fabrication of silver helix microstructures in a large area by a two-photon absorption DLW method

EDX spectrum of the SU-8 surface after electroless silver plating. (a) Before plating at t = 0 min. (b) After 5 min of plating. (c) After 10 min of plating. (d) After 30 min of plating. (e) After 60 min of plating. (f) Plot of the peak ratio between Ag and C as a function of plating time.