Figure 4
From: Corrosion behavior of X80 pipeline steel local defect pits under static liquid film

EIS spectra for sample with ADP under static liquid film, h = 2.5 mm: (a) Nyquist plots, (b) Bode and |Z| plots.
From: Corrosion behavior of X80 pipeline steel local defect pits under static liquid film
EIS spectra for sample with ADP under static liquid film, h = 2.5 mm: (a) Nyquist plots, (b) Bode and |Z| plots.