Table 3 EDS test element content inside and outside defect of defect samples under static liquid film (atom %).
From: Corrosion behavior of X80 pipeline steel local defect pits under static liquid film
Area | h (mm) | C K | O K | Si K | Mn K | Fe K | Mo k |
---|---|---|---|---|---|---|---|
a | 1 | 25.99 | 9.55 | 0.89 | 1.24 | 62.14 | 0.19 |
2.5 | 25.48 | 10.29 | 0.72 | 1.20 | 62.09 | 0.22 | |
4.5 | 23.02 | 9.12 | 1.24 | 1.46 | 64.97 | 0.19 | |
6 | 27.43 | 11.01 | 1.23 | 1.29 | 58.94 | 0.09 | |
8 | 26.34 | 8.78 | 1.08 | 1.21 | 62.31 | 0.28 | |
b | 1 | 17.65 | 12.83 | 1.07 | 1.23 | 66.99 | 0.22 |
2.5 | 19.31 | 11.07 | 0.67 | 1.30 | 67.51 | 0.13 | |
4.5 | 20.42 | 10.68 | 1.14 | 1.39 | 66.23 | 0.13 | |
6 | 21.09 | 9.57 | 1.14 | 1.48 | 66.51 | 0.20 | |
8 | 25.18 | 10.94 | 1.18 | 1.22 | 61.30 | 0.18 |