Table 1 The corresponding data derived from the GC testing.
Samples | Current density at 120 min (μA/cm2) | Electrode potential at 120 min (V) | Current density reduced up to 120 min (%) |
---|---|---|---|
Al 7075 T6 | 58.2 | − 0.69 | – |
TFSAA | 51.5 | − 0.56 | 12 |
PEO-300 | 36.6 | − 0.58 | 59 |
PEO-500 | 9.7 | − 0.55 | 83 |
PEO-600 | 6.1 | − 0.42 | 90 |