Figure 5
From: Processing of high temperature alumina/aluminum titanate ceramic composites from clean sources

FE-SEM micrographs of the sintered A/AT composites with different rutile content (0–40 wt%).
From: Processing of high temperature alumina/aluminum titanate ceramic composites from clean sources

FE-SEM micrographs of the sintered A/AT composites with different rutile content (0–40 wt%).