Figure 4

The normalized magnetization (M/Ms) vs magnetic field H for NFO/MGO (100) with thicknesses of (a) 2.5 μm and (b) 16 μm for in-plane H along [001] direction and for out-of-plane H along [100]. Similar M/Ms vs H data for NFO/MGO (110) with thicknesses of (c) 5 μm and (d) 10 μm for in-plane H along [001] and [1\(\overline{1}\)0] directions and for out-of-plane H along [110] direction.