Figure 10

Strain induced resistance change upon applying the sensor on mice body (a), sensor resistance change is measured while it is elongated to 50% using a stretch bench and maintained it in the same position for 24 h (a, insets). Thermoelectric voltage generated during the test period of 4–12 days and corresponding ΔT is also shown in b.